Export this record: EndNote BibTex

Please use this identifier to cite or link to this item: https://tede2.pucrs.br/tede2/handle/tede/11592
Full metadata record
DC FieldValueLanguage
dc.creatorPolicarpi, Taila Cristiane-
dc.contributor.advisor1Moehlecke, Adriano-
dc.contributor.advisor-co1Zanesco, Izete-
dc.date.accessioned2025-05-13T14:17:19Z-
dc.date.issued2024-05-27-
dc.identifier.urihttps://tede2.pucrs.br/tede2/handle/tede/11592-
dc.description.resumoO decréscimo da potência dos módulos fotovoltaicos (FV) após a instalação pode ocorrer pela degradação sofrida pelo módulo, que depende, entre outros fatores, da estrutura da célula solar, dos materiais utilizados na fabricação do módulo FV e do ambiente. O presente trabalho analisa e compara módulos FVs com células solares de tecnologia Al-BSF, de silício multi e monocristalino (Si-Mc e Si-mono), instalados em três propriedades rurais no oeste do Paraná. Módulos FVs de teste foram inseridos nos sistemas, bem como módulos de referência foram armazenados, sendo caracterizados eletricamente após períodos de operação/armazenamento, permitindo avaliar a evolução dos parâmetros elétricos e, por meio deles, a taxa de degradação, assim como o efeito da sujidade nos módulos FVs de teste em operação. Antes da instalação nas propriedades rurais, a caracterização elétrica dos módulos FVs revelou potências superiores às nominais. Após o período de exposição, a degradação para os módulos de Si-Mc ficou no intervalo de -4,4% a -5,0% (em 3 anos) e para os de Si mono foi de -1,7% (2 anos), divergindo das previsões do fabricante que são da ordem de -3,7 % para os módulos FVs de Si-Mc (em 3 anos) e de 3,5% para os módulos FVs de Si-mono (2 anos). Os módulos FVs de Si-Mc armazenados apresentaram uma queda de potência da ordem de -2,4% e -3,5 % (para potência nominal de 270 Wp e 325 Wp, respectivamente) enquanto os de Si-mono mostraram uma queda de somente -0,8%. A degradação estimada pelo desempenho global dos sistemas FVs foi similar a calculada por meio dos parâmetros elétricos somente para os módulos FVs com menor acúmulo de sujidade.por
dc.description.abstractThe decrease in the power of photovoltaic (PV) modules after installation can occur due to the degradation suffered by the module, which depends, among other factors, on the structure of the solar cell, the materials used in the manufacture of the PV module and the environment. The present work analyzes and compares PV modules with Al-BSF technology solar cells, multi and monocrystalline silicon (Si-Mc and Si mono, respectively), installed in three rural properties in the west of Paraná. Test PV modules were installed into the PV systems and reference modules were stored, being electrically characterized after periods of operation/storage, allowing to evaluate the evolution of the electrical parameters and through them the degradation rate, as well as the effect of soiling on the test PV modules in operation. Prior to the installation in the rural properties, the electrical characterization of the PV modules revealed higher nominal powers than those specified by manufacturer datasheet. After the exposure period, the degradation for Si-Mc modules was in the range of -4.4% to -5.0% (in 3 years) and for Si-mono modules was -1.7% (2 years), differing from the manufacturer's forecasts of -3.7% for Si-Mc PV modules (in 3 years) and 3.5% for Si-mono PV modules (2 years). The stored Si-Mc PV modules showed a power drop of -2.4% and -3.5% (for rated power of 270 Wp and 325 Wp, respectively) while the Si-mono modules showed a decrease of only -0.8%. The degradation estimated by the performance ratio of the PV systems was similar to that calculated through the electrical parameters solely for the PV modules with lower soiling.eng
dc.description.provenanceSubmitted by PPG Engenharia e Tecnologia de Materiais ([email protected]) on 2025-05-13T12:46:05Z No. of bitstreams: 1 Taila_Cristiane_Policarpi_TES.pdf: 10830579 bytes, checksum: 67b2c5ca5757eba5fa319fb4d7af2f44 (MD5)eng
dc.description.provenanceApproved for entry into archive by Sheila Dias ([email protected]) on 2025-05-13T14:00:27Z (GMT) No. of bitstreams: 1 Taila_Cristiane_Policarpi_TES.pdf: 10830579 bytes, checksum: 67b2c5ca5757eba5fa319fb4d7af2f44 (MD5)eng
dc.description.provenanceMade available in DSpace on 2025-05-13T14:17:19Z (GMT). No. of bitstreams: 1 Taila_Cristiane_Policarpi_TES.pdf: 10830579 bytes, checksum: 67b2c5ca5757eba5fa319fb4d7af2f44 (MD5) Previous issue date: 2024-05-27eng
dc.description.sponsorshipCoordenação de Aperfeiçoamento de Pessoal de Nível Superior - CAPESpor
dc.formatapplication/pdf*
dc.thumbnail.urlhttps://tede2.pucrs.br/tede2/retrieve/193365/Taila_Cristiane_Policarpi_TES.pdf.jpg*
dc.languageporpor
dc.publisherPontifícia Universidade Católica do Rio Grande do Sulpor
dc.publisher.departmentEscola Politécnicapor
dc.publisher.countryBrasilpor
dc.publisher.initialsPUCRSpor
dc.publisher.programPrograma de Pós-Graduação em Engenharia e Tecnologia de Materiaispor
dc.rightsAcesso Abertopor
dc.subjectMódulos Fotovoltaicospor
dc.subjectDegradaçãopor
dc.subjectCélulas Solares de Silíciopor
dc.subjectPhotovoltaic Moduleseng
dc.subjectDegradationeng
dc.subjectSilicon Solar Cellseng
dc.subject.cnpqENGENHARIASpor
dc.subject.cnpqMATERIAIS ELETRICOS::MATERIAIS E COMPONENTES SEMICONDUTORESpor
dc.titleRedução da potência em módulos fotovoltaicos : análise dos parâmetros elétricos iniciais e da degradação dos primeiros anos em condições externaspor
dc.typeTesepor
dc.restricao.situacaoTrabalho não apresenta restrição para publicaçãopor
Appears in Collections:Programa de Pós-Graduação em Engenharia e Tecnologia de Materiais

Files in This Item:
File Description SizeFormat 
Taila_Cristiane_Policarpi_TES.pdfTAILA_CRISTIANE_POLICARPI_TES10.58 MBAdobe PDFThumbnail

Download/Open Preview


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.